Kiilto Pro WRX 3071
Kiilto Pro WRX 3071 is an EN 204 D3 classified PVAC wood adhesive for veneering and lamination.
Special features
- non-discoloring
- very fast bonding
- does not bleed through in veneering
- includes renewable raw materials
Links
Materials
Kiilto Pro WRX 3071 is a very fast bonding reactive PVAc-dispersion adhesive with neutral pH. Suitable for veneering as well as foil lamination of solid wood, parquet, bathroom fixture, laminate and wood based boards with a hot press. Thanks to its D3 water resistance level, Kiilto Pro WRX 3071 is suitable for both interior and exterior applications that have repetitive short-term contact with water.
Package Size | Product Code |
---|---|
Kiilto Pro WRX 3071 15 kg | T1458.015 |
Kiilto Pro WRX 3071 IBC cont | T1458.994 |
8%
PVAc
PVAc
ca. 1,2 kg/dm³.
7 - 8
Light colour, translucent when dry.
10 000 mPas (Brookfield RVT +20 °C)
120–150 g/m² (solid wood)
80–100 g/m² (veneering and foil lamination)
Hot pressing, look at the table
0,5 N/mm²
+10 - +30 °C
+3 °C
6 - 15 %
Can be stored in unopened containers, above +1 °C, for 4 months. After long storing, stir before use.
The adhesive should not be mixed with other PVAc adhesives, the production line must be cleaned before using this adhesive.
Check that the joints fit well. Apply adhesive one-sided in an even layer. Assemble and press the parts together aiming at an even squeeze out for the whole length of the joint. The joints can be pressed in a cold or hot press. The final strength and water resistance of the bond is reached within 7 days.
The open time of the adhesive depends on the amount of adhesive used (pine 12 % wood moisture, 23 °C, 50 % RH):
Amount of adhesive (g/m²) | Open time (minutes) |
80 | 2 |
100 | 3 |
120 | 4 |
150 | 6 |
Pressing time in veneering with adhesive amount 100 g/m²
Pressing temperature (°C) | Pressing time (sec) |
60 | 60 |
70 | 50 |
80 | 40 |
The information given in this product data sheet is based on our tests and our practical knowledge. The technical data is defined in standard conditions. Variations in local working conditions will affect the product performance and result. The result is also strongly affected by working methods. We guarantee the high quality of our products according to our Quality Management System. No liability can be accepted from incorrect use of the product or prevailing conditions, over which we have no control. Thus, we cannot be held responsible for the final result. The user of the product must test the product’s suitability for the intended application.
Avoid unnecessary skin contact and exposure with the fresh product, use safety gloves. Refer to material safety data sheet. For information on product and package disposal, visit www.kiilto.com.